note it also adds that non magnetic mineralisation can be upgraded 4-5 times.
syrah add that the combination of the two types produced a pre chemical treatment concentrate around 3% from i assume, a resource called at 0.23% V2O5.
We are slightly better than that, at 0.29% overall ,but consider that there might be selective high grade zones to better that again.
Multiply and the chemical pre treatment head grade might be more than syrahs 3%, to produce a end product (syrah quote 99.9% V2O5)
hard to say, but a fair assumption to treat as similar to syrahs at this stage.